IMI Alloy India LLP is a familiar stockist of HSS M35 Turning Scrap. We are also a provider, manufacturer, and exporter of HSS M35 Turning Scrap. Our company only uses certified raw materials for manufacturing. For suitable suppliers, our company buys this raw material. Our company has a highly qualified employee team who always works hard to produce these turning scraps with exclusive quality. Our experts keep controls on the production process from raw material to the final product. As a result, our HSS M35 Turning Scrap can stay at a high temperature without any damage. This turning scrap is used in the automobile Industry, Construction, Pharmaceutical, and Chemical Industry, Oil and Gas industries. M35 is a cobalt high speed steel alloy.
Our HSS M35 Turning Scraps has some features, such as all-around working applicability, good machine ability, good performance, and good hot hardness, which are unique in industries. HSS M35 is excellent coordination of toughness and hardness.
Table of Content
In chemical composition, cobalt content increases the hardness. Our HSS M35 Turing Scrap has suitable thicknesses, modulus of flexibility, co-efficient of thermal extension, and specific heat. Due to HSS M35 Turning Scraps offer excellent performance and properties, it is used in cutting conditions where hot hardness is required. HSS M35 turning Scrap is ideal for cold working where wear resistance is needed. HSS M35 Turning Scrap shows the commendable combination of wear resistance and toughness.
Country | USA | German | Japan |
Standard | – | DIN EN ISO 4957 | JIS G4403 |
Grades | M35 | 1.3243/HS6-5-2-5 | SKH55 |
ASTM | C | Mn | P | S | Si | Cr | V | Mo | W | Co | ||||||||
M35 | 0.82 | 0.95 | 0.15 | 0.40 | 0.03 | 0.03 | 0.20 | 0.45 | 3.80 | 4.50 | 1.75 | 2.15 | 4.75 | 5.25 | 5.50 | 6.50 | 4.60 | 5.00 |
DIN ISO 4957 | C | Mn | P | S | Si | Cr | V | Mo | W | Co | ||||||||
1.3243/HS6-5-2-5 | 0.87 | 0.95 | … | 0.40 | 0.03 | 0.03 | … | 0.45 | 3.80 | 4.50 | 1.70 | 2.10 | 4.70 | 5.20 | 5.90 | 6.70 | 4.50 | 5.00 |
JIS G4403 | C | Mn | P | S | Si | Cr | V | Mo | W | Co | ||||||||
SKH55 | 0.87 | 0.95 | … | 0.40 | 0.03 | 0.03 | … | 0.45 | 3.80 | 4.50 | 1.70 | 2.10 | 4.70 | 5.20 | 5.90 | 6.70 | 4.50 | 5.00 |
Temperature °C / °F | |||||||
20 / 70 | 400 / 750 | 600 / 1110 | |||||
Density | Kg/m³ lbs/in³ | 8150 .294 | 8050 .290 | 7990 .228 | |||
Modulus of Elasticity | kN/mm³² psi | 230 34 · 10 6 | 205 31 · 10 6 | 184 27 · 10 6 | |||
Coefficient of Thermanl expansion from 20°C / 70°F | per °C per °F | – | 11.6 · 10-6 6.4 · 10-6 | 11.9 · 10-6 6.6 · 10-6 | |||
Thermal Conductivity | W/m °C Btu/sq. ft. h °F/in. | 24 166 | 28 194 | 27 187 | |||
Specific Heat | J/kg °C Btu/lb °F | 420 0.10 | 510 0.12 | 600 0.14 |
Mechanical properties | Metric | Imperial |
Hardness, Rockwell C (oil quenched from 1232°C, 5 mins) | 64.8 | 64.8 |
Hardness, Rockwell C (oil quenched from 1177°C, 5 mins) | 65.2 | 65.2 |
Hardness, Rockwell C (oil quenched from 1204°C, 5 mins) | 65.2 | 65.2 |
Modulus of elasticity | 207 GPa | 30000 ksi |
Machinability (1% carbon steel) | 45.0 – 50.0% | 45.0 – 50.0% |
Thermal properties | Metric | Imperial |
CTE, linear (@21 – 399°C / 69.8 – 750°F) | 11.4 μm/m°C | 6.33 μin/in°F |
CTE, linear (@21 – 593°C /69.8 – 1100°F) | 11.5 μm/m°C | 6.39 μin/in°F |
Generally, high speed steels are used for machining at high speeds. HSS M35 steel materials are widely used for: